1.powder brand: 316L, 304, 17-4PH, M2, CAM-J55, Ni55, Ni60, GH3635, GH4169, GH3625, GH5188, TC4, TA15, CoCrW, CoCrMo;
2.Powder characteristics: good sphericity, low oxygen content, uniform particle size distribution, high batch stability, good fluidity and high loose density and vibration density.
3.powder application: Powder can be used in laser/electron beam additive manufacturing (SLM/EBM), powder metallurgy (PM), laser direct deposition (DLD), powder hot isostatic pressing (HIP), metal injection molding (MIM) and other processes. It is widely used in aerospace, petrochemical, nuclear reactor, laser cladding and other fields.
4.product specifications: 0-45μm, 15-45μm, 15-53μm, 45-150μm. (can be customized according to customer requirements)